Z3CND17-11-01 Stainless Steels to NF A 35-573

Z3CND17-11-01 - Specification & Application

  • NF A 35-573 - Stainless steels for general purposes. Plates, wide strips and strips

Stainless steels for general purposes. Plates, wide strips and strips

Chemical composition(wt.%) of Z3CND17-11-01 grade: to NF A 35-573

Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.030
Si - 1.00
Mn - 2.00
P - 0.040
S - 0.030
Cr 16.00 18.00
Mo 0.90 1.10
Ni 10.00 12.00

Z3CND17-11-01 - Detail

Stainless steels for general purposes. Plates, wide strips and strips

Mechanical properties of grade Z3CND17-11-01 NF A 35-573

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
759 (≥) 259 (≥) 11 42 33 Solution and Aging, Annealing, Ausaging, Q+T,etc 232

Physical properties of grade Z3CND17-11-01 NF A 35-573

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
258 (≥) 721 (≥) 12 24 31 Solution and Aging, Annealing, Ausaging, Q+T,etc 244
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
319 116 916

Equivalent Grade

Equivalent Products

We can customize the production of Z3CND17-11-01 grade, contact us for the best solution.
sales@specificsteel.com