Z3CND17-11-02FF Stainless Steels to NF A 35-577

Z3CND17-11-02FF - Specification & Application

  • NF A 35-577 - Iron and steel. Stainless steel wire rods for cold forming

Iron and steel. Stainless steel wire rods for cold forming

Chemical composition(wt.%) of Z3CND17-11-02FF grade: to NF A 35-577

Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.030
Si - 0.70
Mn 0.30 1.00
P - 0.040
S - 0.010
Cr 16.50 17.50
Mo 2.00 2.50
Ni 11.00 12.00

Z3CND17-11-02FF - Detail

Iron and steel. Stainless steel wire rods for cold forming

Mechanical properties of grade Z3CND17-11-02FF NF A 35-577

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
535 (≥) 182 (≥) 21 14 33 Solution and Aging, Annealing, Ausaging, Q+T,etc 123

Physical properties of grade Z3CND17-11-02FF NF A 35-577

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
284 (≥) 266 (≥) 14 11 31 Solution and Aging, Annealing, Ausaging, Q+T,etc 342
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
174 833 793