Z4C17FF Stainless Steels to NF A 35-577

Z4C17FF - Specification & Application

  • NF A 35-577 - Iron and steel. Stainless steel wire rods for cold forming

Iron and steel. Stainless steel wire rods for cold forming

Chemical composition(wt.%) of Z4C17FF grade: to NF A 35-577

Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.040
Si - 1.00
Mn - 1.00
P - 0.040
S - 0.015
Cr 16.00 18.00
Mo - 0.30
Ni - 0.50

Z4C17FF - Detail

Iron and steel. Stainless steel wire rods for cold forming

Mechanical properties of grade Z4C17FF NF A 35-577

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
994 (≥) 581 (≥) 14 14 22 Solution and Aging, Annealing, Ausaging, Q+T,etc 433

Physical properties of grade Z4C17FF NF A 35-577

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
898 (≥) 667 (≥) 33 43 21 Solution and Aging, Annealing, Ausaging, Q+T,etc 244
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
494 957 329

Equivalent Grade

Equivalent Products

We can customize the production of Z4C17FF grade, contact us for the best solution.