Z5CN18-11FF Stainless Steels to NF A 35-577

Z5CN18-11FF - Specification & Application

  • NF A 35-577 - Iron and steel. Stainless steel wire rods for cold forming

Iron and steel. Stainless steel wire rods for cold forming

Chemical composition(wt.%) of Z5CN18-11FF grade: to NF A 35-577

Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.050
Si - 0.70
Mn 0.30 1.00
P - 0.040
S - 0.010
Cr 17.50 18.50
Mo - -
Ni 10.80 11.80

Z5CN18-11FF - Detail

Iron and steel. Stainless steel wire rods for cold forming

Mechanical properties of grade Z5CN18-11FF NF A 35-577

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
827 (≥) 775 (≥) 14 44 43 Solution and Aging, Annealing, Ausaging, Q+T,etc 111

Physical properties of grade Z5CN18-11FF NF A 35-577

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
875 (≥) 439 (≥) 24 13 14 Solution and Aging, Annealing, Ausaging, Q+T,etc 332
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
933 178 761

Equivalent Grade

Equivalent Products

We can customize the production of Z5CN18-11FF grade, contact us for the best solution.
sales@specificsteel.com