Z60CMDVNb21-10Az Stainless Steels to NF A 35-579

Z60CMDVNb21-10Az - Specification & Application

  • NF A 35-579 - Valve steels and alloys for internal combustion engines

Valve steels and alloys for internal combustion engines

Chemical composition(wt.%) of Z60CMDVNb21-10Az grade: to NF A 35-579

Elements Min.(≥) Max.(≤) Similar Remarks
C 0.57 0.65
Si - 0.25
Mn 9.50 11.50
P - 0.040
S - 0.030
Cr 20.00 22.00
Ni - 1.50
Mo 0.75 1.25
Nb 1.00 1.20
V 0.75 1.00
N 0.40 0.60

Z60CMDVNb21-10Az - Detail

Valve steels and alloys for internal combustion engines

Mechanical properties of grade Z60CMDVNb21-10Az NF A 35-579

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
992 (≥) 974 (≥) 31 33 32 Solution and Aging, Annealing, Ausaging, Q+T,etc 342

Physical properties of grade Z60CMDVNb21-10Az NF A 35-579

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
425 (≥) 676 (≥) 13 41 31 Solution and Aging, Annealing, Ausaging, Q+T,etc 134
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
535 823 319

Equivalent Products

We can customize the production of Z60CMDVNb21-10Az grade, contact us for the best solution.