Z6CNDT17-13B Stainless Steels to NF A 35-578

Z6CNDT17-13B - Specification & Application

  • NF A 35-578 - Iron and steel. Stainless steel for high temperature application

Iron and steel. Stainless steel for high temperature application

Chemical composition(wt.%) of Z6CNDT17-13B grade: to NF A 35-578

Elements Min.(≥) Max.(≤) Similar Remarks
C 0.04 0.08
Si - 0.75
Mn - 2.00
P - 0.040
S - 0.015
Cr 16.00 18.00
Mo 12.00 14.00
Ni - -
B 0.0015 0.0060
Ti 4(C+N) 0.70

Z6CNDT17-13B - Detail

Iron and steel. Stainless steel for high temperature application

Mechanical properties of grade Z6CNDT17-13B NF A 35-578

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
123 (≥) 199 (≥) 44 14 23 Solution and Aging, Annealing, Ausaging, Q+T,etc 213

Physical properties of grade Z6CNDT17-13B NF A 35-578

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
385 (≥) 853 (≥) 24 11 41 Solution and Aging, Annealing, Ausaging, Q+T,etc 141
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
976 875 452

Equivalent Grade

Equivalent Products

We can customize the production of Z6CNDT17-13B grade, contact us for the best solution.