Z6CNUD15-04 Air 9160/C Aviation and Aero Steel to AIR 9160 C

Z6CNUD15-04 Air 9160/C - Specification & Application

  • AIR 9160 C - wrought steels used in aeronautical constructions

wrought steels used in aeronautical constructions

Chemical composition(wt.%) of Z6CNUD15-04 Air 9160/C grade: to AIR 9160 C

Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.07
Si - 1.00
Mn - 1.00
P - 0.035
S - 0.025
Cr 13.50 15.50
Ni 3.00 5.00
Mo 1.00 1.60
Cu 2.50 4.50

Z6CNUD15-04 Air 9160/C - Detail

Z6CNUD15-04 Air 9160C wrought steels used in aeronautical constructions

Mechanical properties of grade Z6CNUD15-04 Air 9160/C AIR 9160 C

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
279 (≥) 866 (≥) 24 42 14 Solution and Aging, Annealing, Ausaging, Q+T,etc 332

Physical properties of grade Z6CNUD15-04 Air 9160/C AIR 9160 C

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
686 (≥) 369 (≥) 21 12 24 Solution and Aging, Annealing, Ausaging, Q+T,etc 132
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
377 585 831

Equivalent Grade

Equivalent Products

We can customize the production of Z6CNUD15-04 Air 9160/C grade, contact us for the best solution.