Z8C17 Stainless Steels to NF A 35-573

Z8C17 - Specification & Application

  • NF A 35-573 - Stainless steels for general purposes. Plates, wide strips and strips
  • NF A 35-574 - Iron and steel. Stainless steel for general purposes. Semi- finished products, bars and wire rod
  • NF A 35-578 - Iron and steel. Stainless steel for high temperature application
  • NF F 80-109 - Rolling stock. Recommanded steels for rolling stock construction. IX: stainless steels for general purposes

Rolling stock. Recommanded steels for rolling stock construction. IX: stainless steels for general purposes

Chemical composition(wt.%) of Z8C17 grade: to NF A 35-573

Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.080
Si - 0.75
Mn - 0.75
P - 0.040
S - 0.015
Cr 16.00 17.50
Mo - -
Ni - -

Z8C17 - Detail

Rolling stock. Recommanded steels for rolling stock construction. IX: stainless steels for general purposes

Mechanical properties of grade Z8C17 NF A 35-573

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
663 (≥) 351 (≥) 14 31 44 Solution and Aging, Annealing, Ausaging, Q+T,etc 334

Physical properties of grade Z8C17 NF A 35-573

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
911 (≥) 522 (≥) 11 23 13 Solution and Aging, Annealing, Ausaging, Q+T,etc 433
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
447 366 819

Equivalent Products

We can customize the production of Z8C17 grade, contact us for the best solution.