Steel tubes. Seamless austenitic steel tubes for use at high temperatures. Dimensions (with normal tolerances). Technical conditions of delivery
Elements | Min.(≥) | Max.(≤) | Similar | Remarks |
---|---|---|---|---|
C | 0.05 | 0.10 | ||
Si | - | 1.00 | ||
Mn | - | 2.00 | ||
P | - | 0.040 | ||
S | - | 0.030 | ||
Cr | 16.00 | 18.00 | ||
Ni | 12.00 | 14.00 | ||
Mo | 2.00 | 2.50 | ||
B | 0.0015 | 0.0060 | ||
Ti | 4×C | 0.70 |
Steel tubes. Seamless austenitic steel tubes for use at high temperatures. Dimensions (with normal tolerances). Technical conditions of delivery
Proof strength Rp0.2 (MPa) |
Tensile strength Rm (MPa) |
Impact energy KV (J) |
Elongation at fracture A (%) |
Reduction in cross section on fracture Z (%) |
As-Heat-Treated Condition | Brinell hardness (HBW) |
---|---|---|---|---|---|---|
147 (≥) | 626 (≥) | 23 | 33 | 22 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 334 |
Property | Density kg/dm3 |
Temperature T °C/F |
Specific heat J / kgK |
Thermal conductivity W/mK |
Electric resistance µΩ·cm |
Modulus of elasticity kN/mm2 |
Expansion rate |
---|---|---|---|---|---|---|---|
656 (≥) | 274 (≥) | 33 | 31 | 21 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 122 | |
Temp. °C/°F |
Creep strain limit (10000h) (Rp1,0) N/mm2 |
Creep rupture strength (10000h) (Rp1,0) N/mm2 |
|||||
484 | 775 | 425 |
We can customize the production of Z8CNDT17.13B grade, contact us for the best solution.
–sales@specificsteel.com