Z9CNDA15-07 Stainless Steels to NF A 35-574

Z9CNDA15-07 - Specification & Application

  • NF A 35-574 - Iron and steel. Stainless steel for general purposes. Semi- finished products, bars and wire rod

Iron and steel. Stainless steel for general purposes. Semi- finished products, bars and wire rod

Chemical composition(wt.%) of Z9CNDA15-07 grade: to NF A 35-574

Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.090
Si - 0.75
Mn - 1.00
P - 0.040
S - 0.025
Cr 14.00 16.00
Mo 2.00 3.00
Ni 6.50 7.50
Al 0.75 1.50

Z9CNDA15-07 - Detail

Iron and steel. Stainless steel for general purposes. Semi- finished products, bars and wire rod

Mechanical properties of grade Z9CNDA15-07 NF A 35-574

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
544 (≥) 639 (≥) 42 13 14 Solution and Aging, Annealing, Ausaging, Q+T,etc 343

Physical properties of grade Z9CNDA15-07 NF A 35-574

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
947 (≥) 453 (≥) 41 13 43 Solution and Aging, Annealing, Ausaging, Q+T,etc 334
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
295 686 428

Equivalent Grade

Equivalent Products

We can customize the production of Z9CNDA15-07 grade, contact us for the best solution.