ЭИ835 Stainless Steels

ЭИ835 - Specification & Application

Russia GOCT Standard vacuum smelting casting high temperature alloy bar

Chemical composition(wt.%) of ЭИ835 grade:

Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.12
Si - 1.00
Mn 5.00 7.00
P - 0.035
S - 0.020
Cr 23.00 26.00
Mo - -
Ni 15.00 18.00
N 0.30 0.45
B - 0.010

ЭИ835 - Detail

Russia GOCT Standard vacuum smelting casting high temperature alloy bar

Mechanical properties of grade ЭИ835

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
135 (≥) 686 (≥) 14 13 14 Solution and Aging, Annealing, Ausaging, Q+T,etc 122

Physical properties of grade ЭИ835

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
824 (≥) 324 (≥) 42 12 12 Solution and Aging, Annealing, Ausaging, Q+T,etc 111
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
177 928 966

Equivalent Products

We can customize the production of ЭИ835 grade, contact us for the best solution.
sales@specificsteel.com