X21CrMoNiV12-2 Stainless Steels to ISO/TR 4956

X21CrMoNiV12-2 - Specification & Application

  • ISO/TR 4956 - Wrought steels for use at elevated temperatures in engines

Wrought steels for use at elevated temperatures in engines

Chemical composition(wt.%) of X21CrMoNiV12-2 grade: to ISO/TR 4956

Elements Min.(≥) Max.(≤) Similar Remarks
C 0.17 0.25
Si - 0.50
Mn - 1.00
P - 0.035
S - 0.030
Cr 11.00 12.50
Mo 0.70 1.20
Ni 0.30 1.00
V 0.20 0.35

X21CrMoNiV12-2 - Detail

Wrought steels for use at elevated temperatures in engines

Mechanical properties of grade X21CrMoNiV12-2 ISO/TR 4956

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
414 (≥) 537 (≥) 24 43 44 Solution and Aging, Annealing, Ausaging, Q+T,etc 112

Physical properties of grade X21CrMoNiV12-2 ISO/TR 4956

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
616 (≥) 547 (≥) 14 23 44 Solution and Aging, Annealing, Ausaging, Q+T,etc 142
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
743 699 484

Equivalent Products

We can customize the production of X21CrMoNiV12-2 grade, contact us for the best solution.
sales@specificsteel.com