Specification for nickel-copper alloy castings
Elements | Min.(≥) | Max.(≤) | Similar | Remarks |
---|---|---|---|---|
C | - | 0.15 | ||
Si | 2.00 | 3.00 | ||
Mn | - | 1.50 | ||
P | - | 0.030 | ||
S | - | 0.030 | ||
Cr | - | - | ||
Mo | - | - | ||
Ni | - | remaining | ||
Cu | 28.00 | 34.00 |
Specification for nickel-copper alloy castings
Proof strength Rp0.2 (MPa) |
Tensile strength Rm (MPa) |
Impact energy KV (J) |
Elongation at fracture A (%) |
Reduction in cross section on fracture Z (%) |
As-Heat-Treated Condition | Brinell hardness (HBW) |
---|---|---|---|---|---|---|
437 (≥) | 396 (≥) | 32 | 43 | 43 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 321 |
Property | Density kg/dm3 |
Temperature T °C/F |
Specific heat J / kgK |
Thermal conductivity W/mK |
Electric resistance µΩ·cm |
Modulus of elasticity kN/mm2 |
Expansion rate |
---|---|---|---|---|---|---|---|
344 (≥) | 921 (≥) | 13 | 23 | 43 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 332 | |
Temp. °C/°F |
Creep strain limit (10000h) (Rp1,0) N/mm2 |
Creep rupture strength (10000h) (Rp1,0) N/mm2 |
|||||
858 | 543 | 487 |
We can customize the production of NA2 grade, contact us for the best solution.
–sales@specificsteel.com