Non magnetizable steels. Technical delivery conditions,Ship building,Electrical engineering,Machine engineering,Resistant in sea water up to approx. 60 °C, also against stress corrosion cracking
Elements | Min.(≥) | Max.(≤) | Similar | Remarks |
---|
Non magnetizable steels. Technical delivery conditions
Proof strength Rp0.2 (MPa) |
Tensile strength Rm (MPa) |
Impact energy KV (J) |
Elongation at fracture A (%) |
Reduction in cross section on fracture Z (%) |
As-Heat-Treated Condition | Brinell hardness (HBW) |
---|---|---|---|---|---|---|
538 (≥) | 818 (≥) | 32 | 13 | 42 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 244 |
Property | Density kg/dm3 |
Temperature T °C/F |
Specific heat J / kgK |
Thermal conductivity W/mK |
Electric resistance µΩ·cm |
Modulus of elasticity kN/mm2 |
Expansion rate |
---|---|---|---|---|---|---|---|
156 (≥) | 186 (≥) | 34 | 34 | 24 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 323 | |
Temp. °C/°F |
Creep strain limit (10000h) (Rp1,0) N/mm2 |
Creep rupture strength (10000h) (Rp1,0) N/mm2 |
|||||
897 | 775 | 894 |
We can customize the production of 1-3974 / F49 / S33228 / X2CrNiMnMoNNb23-17-6-3 grade, contact us for the best solution.