1.4406 Stainless Steels to BS EN 10028-7

1.4406 - Specification & Application

  • BS EN 10028-7 - Flat products made of steels for pressure purposes - Part 7: Stainless steels
  • BS EN 10088-1 - Stainless steels - Part 1: List of stainless steels
  • BS EN 10088-2 - Stainless steels - Part 2: Technical delivery conditions for sheet/plate and strip of corrosion resisting steels for general purposes
  • BS EN 10088-3 - Stainless steels - Part 3: Technical delivery conditions for semi-finished products, bars, rods, wire, sections and bright products of corrosion resisting steels for general purposes
  • BS EN 10088-4 - Stainless steels - Part 4: Technical delivery conditions for sheet/plate and strip of corrosion resisting steels for construction purposes
  • BS EN 10088-5 - Stainless steels - Part 5: Technical delivery conditions for bars, rods, wire, sections and bright products of corrosion resisting steels for construction purposes
  • BS EN 10222-5 - Steel forgings for pressure purposes - Part 5: Martensitic, austenitic and austenitic-ferritic stainless steels
  • BS EN 10250-4 - Open die steel forgings for general engineering purposes - Part 4: Stainless steels
  • BS EN 10272 - Stainless steel bars for pressure purposes

Stainless steel bars for pressure purposes

Chemical composition(wt.%) of 1.4406 grade: to BS EN 10028-7

Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.03
Si - 1.00
Mn - 2.00
P - 0.045
S - 0.015
Cr 16.50 18.50
Ni 10.00 12.00
Mo 2.00 2.50
N 0.12 0.22

1.4406 - Detail

Stainless steel bars for pressure purposes

Mechanical properties of grade 1.4406 BS EN 10028-7

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
288 (≥) 384 (≥) 14 31 33 Solution and Aging, Annealing, Ausaging, Q+T,etc 414

Physical properties of grade 1.4406 BS EN 10028-7

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
656 (≥) 164 (≥) 21 22 33 Solution and Aging, Annealing, Ausaging, Q+T,etc 322
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
744 822 784