Stainless steel bars for pressure purposes
Elements | Min.(≥) | Max.(≤) | Similar | Remarks |
---|---|---|---|---|
C | - | 0.03 | ||
Si | - | 1.00 | ||
Mn | - | 2.00 | ||
P | - | 0.045 | ||
S | - | 0.015 | ||
Cr | 16.50 | 18.50 | ||
Ni | 10.00 | 12.00 | ||
Mo | 2.00 | 2.50 | ||
N | 0.12 | 0.22 |
Stainless steel bars for pressure purposes
Proof strength Rp0.2 (MPa) |
Tensile strength Rm (MPa) |
Impact energy KV (J) |
Elongation at fracture A (%) |
Reduction in cross section on fracture Z (%) |
As-Heat-Treated Condition | Brinell hardness (HBW) |
---|---|---|---|---|---|---|
922 (≥) | 384 (≥) | 22 | 22 | 12 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 311 |
Property | Density kg/dm3 |
Temperature T °C/F |
Specific heat J / kgK |
Thermal conductivity W/mK |
Electric resistance µΩ·cm |
Modulus of elasticity kN/mm2 |
Expansion rate |
---|---|---|---|---|---|---|---|
183 (≥) | 424 (≥) | 33 | 32 | 11 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 134 | |
Temp. °C/°F |
Creep strain limit (10000h) (Rp1,0) N/mm2 |
Creep rupture strength (10000h) (Rp1,0) N/mm2 |
|||||
991 | 365 | 292 |
We can customize the production of X2CrNiMoN17-11-2 grade, contact us for the best solution.
–sales@specificsteel.com