A 314 S24100 Stainless Steels to A 314 (2008)

A 314 S24100 - Specification & Application

  • A 314 (2008) - Stainless Steel Billets and Bars for Forging

Stainless Steel Billets and Bars for Forging

Chemical composition(wt.%) of A 314 S24100 grade: to A 314 (2008)

Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.15
Mn 11.0 14.0
P - 0.045
S - 0.030
Si - 1.00
Ni 0.5 2.5
Cr 16.5 19.00
N 0.20 0.45

A 314 S24100 - Detail

A 314 S24100

Mechanical properties of grade A 314 S24100 A 314 (2008)

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
285 (≥) 175 (≥) 42 21 41 Solution and Aging, Annealing, Ausaging, Q+T,etc 123

Physical properties of grade A 314 S24100 A 314 (2008)

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
872 (≥) 199 (≥) 33 23 34 Solution and Aging, Annealing, Ausaging, Q+T,etc 244
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
197 833 542

Equivalent Products

We can customize the production of A 314 S24100 grade, contact us for the best solution.
sales@specificsteel.com