H11 Tool Die Steels

H11 - Specification & Application

Hot-Work Tool Steel

Chemical composition(wt.%) of H11 grade:

Elements Min.(≥) Max.(≤) Similar Remarks
C 0.30 0.40
Si 0.80 1.20
Mn 0.20 0.40
Cr 4.75 5.50
Mo 1.25 1.75
V 0.30 0.50
W - -

H11 - Detail

Hot-Work Tool Steel

Mechanical properties of grade H11

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
881 (≥) 125 (≥) 11 24 32 Solution and Aging, Annealing, Ausaging, Q+T,etc 323

Physical properties of grade H11

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
944 (≥) 696 (≥) 33 41 31 Solution and Aging, Annealing, Ausaging, Q+T,etc 233
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
118 272 548
We can customize the production of H11 grade, contact us for the best solution.