O7 Tool Die Steels

O7 - Specification & Application

Oil-Hardening Tool Steel

Chemical composition(wt.%) of O7 grade:

Elements Min.(≥) Max.(≤) Similar Remarks
C 1.10 1.30
Si 0.10 0.60
Mn 0.20 1.00
P - 0.030
S - 0.030
Cr 0.35 0.85
Mo - 0.30
V 0.15 0.40
W 1.00 2.00
Ni+Cu - 0.75

O7 - Detail

Oil-Hardening Tool Steel

Mechanical properties of grade O7

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
916 (≥) 527 (≥) 31 32 43 Solution and Aging, Annealing, Ausaging, Q+T,etc 413

Physical properties of grade O7

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
775 (≥) 875 (≥) 21 11 31 Solution and Aging, Annealing, Ausaging, Q+T,etc 212
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
634 884 833
We can customize the production of O7 grade, contact us for the best solution.