STS XM27 Stainless Steels to D 3749 (2008)

STS XM27 - Specification & Application

  • D 3749 (2008) - Special alloys steel for chemical plant

Special alloys steel for chemical plant

Chemical composition(wt.%) of STS XM27 grade: to D 3749 (2008)

Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.01
Si - 0.40
Mn - 0.40
P - 0.030
S - 0.020
Cr 25.00 27.00
Ni - 0.50
Mo 0.75 1.50
N - 0.015
Cu - 0.20
Ni+Cu - 0.50

STS XM27 - Detail

Special alloys steel for chemical plant

Mechanical properties of grade STS XM27 D 3749 (2008)

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
375 (≥) 229 (≥) 41 13 12 Solution and Aging, Annealing, Ausaging, Q+T,etc 311

Physical properties of grade STS XM27 D 3749 (2008)

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
771 (≥) 591 (≥) 23 31 42 Solution and Aging, Annealing, Ausaging, Q+T,etc 313
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
618 538 543

Equivalent Products

We can customize the production of STS XM27 grade, contact us for the best solution.