STSXM27TB Stainless Steels to D 3577 (2007)

STSXM27TB - Specification & Application

  • D 3577 (2007) - Stainless steel for boiler and heat exchanger tubes

Stainless steel for boiler and heat exchanger tubes

Chemical composition(wt.%) of STSXM27TB grade: to D 3577 (2007)

Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.01
Si - 0.40
Mn - 0.40
P - 0.030
S - 0.020
Cr 25.00 27.00
Ni - 0.50
Mo 0.75 1.50
N - 0.015
Cu - 0.20
Ni+Cu - 0.50

STSXM27TB - Detail

Stainless steel for boiler and heat exchanger tubes

Mechanical properties of grade STSXM27TB D 3577 (2007)

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
394 (≥) 629 (≥) 21 31 33 Solution and Aging, Annealing, Ausaging, Q+T,etc 421

Physical properties of grade STSXM27TB D 3577 (2007)

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
253 (≥) 548 (≥) 31 14 44 Solution and Aging, Annealing, Ausaging, Q+T,etc 221
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
582 456 899

Equivalent Products

We can customize the production of STSXM27TB grade, contact us for the best solution.
sales@specificsteel.com