STS316TB Stainless Steels to D 3577 (2007)

STS316TB - Specification & Application

  • D 3577 (2007) - Stainless steel for boiler and heat exchanger tubes

Stainless steel for boiler and heat exchanger tubes

Chemical composition(wt.%) of STS316TB grade: to D 3577 (2007)

Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.08
Si - 1.00
Mn - 2.00
P - 0.045
S - 0.030
Cr 16.00 18.00
Ni 10.00 14.00
Mo 2.00 3.00
N - -

STS316TB - Detail

Stainless steel for boiler and heat exchanger tubes

Mechanical properties of grade STS316TB D 3577 (2007)

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
534 (≥) 335 (≥) 31 21 21 Solution and Aging, Annealing, Ausaging, Q+T,etc 312

Physical properties of grade STS316TB D 3577 (2007)

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
351 (≥) 397 (≥) 42 14 13 Solution and Aging, Annealing, Ausaging, Q+T,etc 323
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
826 539 573

Equivalent Products

We can customize the production of STS316TB grade, contact us for the best solution.