SUH1 Stainless Steels

SUH1 - Specification & Application

CNS standard heat resistant steel bar steel grade and chemical composition

Chemical composition(wt.%) of SUH1 grade:

Elements Min.(≥) Max.(≤) Similar Remarks
C 0.40 0.50
Si 3.00 3.50
Mn - 0.60
P - 0.030
S - 0.030
Cr 7.50 9.50
Ni - 0.60
Mo - -
N - -
Cu - 0.30

SUH1 - Detail

CNS standard heat resistant steel bar steel grade and chemical composition

Mechanical properties of grade SUH1

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
822 (≥) 345 (≥) 34 14 31 Solution and Aging, Annealing, Ausaging, Q+T,etc 343

Physical properties of grade SUH1

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
896 (≥) 768 (≥) 24 44 23 Solution and Aging, Annealing, Ausaging, Q+T,etc 111
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
181 886 754

Equivalent Grade