XM-18 Stainless Steels to SAE J 405 (1998)

XM-18 - Specification & Application

  • SAE J 405 (1998) - Chemical compositions of SAE wrought stainless steels

Chemical compositions of SAE wrought stainless steels

Chemical composition(wt.%) of XM-18 grade: to SAE J 405 (1998)

Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.03
Si - 0.75
Mn 7.50 9.00
P - 0.045
S - 0.03
Cr 17.5 22.0
Ni 5.00 7.00
Mo 2.00 3.00
N 0.25 0.50

XM-18 - Detail

XM-18

Mechanical properties of grade XM-18 SAE J 405 (1998)

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
977 (≥) 213 (≥) 21 13 43 Solution and Aging, Annealing, Ausaging, Q+T,etc 244

Physical properties of grade XM-18 SAE J 405 (1998)

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
149 (≥) 477 (≥) 23 11 31 Solution and Aging, Annealing, Ausaging, Q+T,etc 211
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
828 845 369

Equivalent Products

We can customize the production of XM-18 grade, contact us for the best solution.