1.0605 Special Alloy

Chemical composition%of the ladle analysis of grade1.0605

C(%)Si(%)Mn(%)P(%)S(%)
0.70-0.800.15-0.350.60-0.800.0450.045
steel with high hardness and high abrasion resistance used for low loaded springs, spring elements, shocks,
some tools and mid loaded parts of machines.

Mechanical properties of grade1.0605

Proof strength
Rp0.2(MPa)
Tensile strength
Rm(MPa)
Impact energy
KV(J)
Elongation at fracture
A(%)
Reduction in cross section on fracture
Z(%)
As-Heat-Treated Condition Brinell hardness(HBW)
462(≥) 115(≥) 14 24 32 Solution and Aging,Annealing,Ausaging,Q+T,etc 333

Physical properties of grade 1.0605

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J/kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
119(≥) 128(≥) 34 41 43 Solution and Aging,Annealing,Ausaging,Q+T,etc 142
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0)N/mm2
Creep rupture strength
(10000h)
(Rp1,0)N/mm2
911 389 446

1.0605 Range of products

Product type Products Dimension Processes Deliver Status
Plates/Sheets Plates/Sheets 0.08-200mm(T)*W*L Forging,hot rolling and cold rolling Annealed,Solution and Aging,Q+T,ACID-WASHED,Shot Blasting
Steel Bar Round Bar,Flat Bar,Square Bar Φ8-1200mm*L Forging,hot rolling and cold rolling,Cast Black,Rough Turning,Shot Blasting,
Coil/Strip Steel Coil/Steel Strip 0.03-16.0x1200mm Cold-Rolled&Hot-Rolled Annealed,Solution and Aging,Q+T,ACID-WASHED,Shot Blasting
Pipes/Tubes Seamless Pipes/Tubes,Welded Pipes/Tubes OD:6-219mm x WT:0.5-20.0mm Hot extrusion,Cold Drawn,Welded Annealed,Solution and Aging,Q+T,ACID-WASHED

1.0605 Steel Stock

Steel grade Dimension Shape Unit Quantity Delivery state Query
SkD-11 Round Bar Stock Φ30-Φ350 Round Bar Kgs 3102 Hot-Rolled+Annealed+black Enquiry
17-4PH Coil Stock 0.08*200mm Coil or Strip Kgs 1623 Cold-Rolled+Annealed Enquiry
17-4PH Round Bar Φ5-300mm*L Round Bar Kgs 46958 Hot-Rolled+Annealed+black Enquiry
17-4PH plate 8-45*1200*3000mm Plate or Sheet Tons 4.9 Hot-Rolled+Annealed+black Enquiry
Cr12MoV 12-160(T)*310-610(W)*L Plate or Sheet Tons 12.38 Hot-Rolled+Annealed+black Enquiry
1.2601 12-160(T)*310-610(W)*L Plate or Sheet Tons 11.22 Hot-Rolled+Annealed+black Enquiry
IncoloyA-286 / GH 2132 Stock Φ8-65mm*L Round Bar Kgs 489 Hot-Rolled+Annealed+black Enquiry
Incoloy800 round bar Φ115*1400 Round Bar Kgs 169 Hot-Rolled+Annealed+black Enquiry
17-7PH / 631 Coil & Strip, Sheet Stock 0.3-3.0*10-180mm Coil or Strip Kgs 1236.22 Cold-Rolled+Annealed Enquiry
X22CrMoV12-1 / 1.4923 Φ17mm Round Bar Kgs 300 Hot-Rolled+Annealed+black Enquiry
1.2083 Forged Plate T:105-185mm*W:510*L Plate or Sheet Tons 26 Forged+QT Enquiry
X22CrMoV12-1 / 1.4923 Φ30mm Round Bar Kgs 300 Hot-Rolled+Annealed+black Enquiry
1.4882 strip/sheet/plate stock 3.5x200x1000-2000mm Coil or Strip Kgs 200 Cold-Rolled+Annealed Enquiry
SA-437 Grade B4B/SUS 616 /422 Forged Bar Dia.160xL Round Bar Kgs 2120 Forged+QT Enquiry
H13 Tool Steel 50x710xL Flat or Square bar PCS 4 Forged+Annealed+black Enquiry
1.2344(H13/X40CrMoV5-1/Z40CDV5) Stock List Dia.182mm - Dia.510mm Round Bar Tons 120 Forged+Annealed+black Enquiry
1.2344 ESR Round Bar Stock List(2019-9-3) Select 0 Select Enquiry
Stainless Steel 422 / Alloy 422 AMS 5655 UNS S42200/616/B4B Round Bar Stock Select 0 Select Enquiry
1.2343 ESR Stock list(2019-09-03) Select 0 Select Enquiry
1.2367 ESR Forged Round Bar stock(2019-09-03) Select 0 Select Enquiry