1.2601 Tool Die Steels

1.2601 - Specification & Application

High alloyed CrMoV steel for cutting tool and cold work tool steel

Chemical composition(wt.%) of 1.2601 grade:

Elements Min.(≥) Max.(≤) Similar Remarks
C 1.55 1.75
Si 0.25 0.40
Mn 0.20 0.40
P - 0.030
S - 0.030
Cr 11.00 12.00
Mo 0.50 0.70
V 0.10 0.50
W 0.40 0.60

1.2601 - Detail

High alloyed CrMoV steel for cutting tool and cold work tool steel

Mechanical properties of grade 1.2601

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
339 (≥) 816 (≥) 22 12 33 Solution and Aging, Annealing, Ausaging, Q+T,etc 324

Physical properties of grade 1.2601

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
814 (≥) 963 (≥) 24 41 44 Solution and Aging, Annealing, Ausaging, Q+T,etc 213
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
815 637 752
We can customize the production of 1.2601 grade, contact us for the best solution.