1.4006 Stainless Steels to DIN 1654-5 (1989)

1.4006 - Specification & Application

  • DIN 1654-5 (1989) - Cold heading and cold extruding steels; technical delivery conditions for stainless steels
  • DIN 17440 (1996) - Stainless steels - Technical delivery conditions for drawn wire
  • DIN 17441 (1985) - Stainless steels - Technical delivery conditions for cold rolled strips and slit coils strip and sheets cut from such strips for pressure purposes
  • DIN 17456 (1985) - Seamless circular tubes of stainless steels for general requirements; technical delivery conditions
  • DIN EN 10088-3 - Stainless steels - Part 3: Technical delivery conditions for semi-finished products, bars, rods, wire, sections and bright products of corrosion resisting steels for general purposes
  • DIN EN 10088-4 - Stainless steels - Part 4: Technical delivery conditions for sheet/plate and strip of corrosion resisting steels for construction purposes
  • DIN EN 10088-5 - Stainless steels - Part 5: Technical delivery conditions for bars, rods, wire, sections and bright products of corrosion resisting steels for construction purposes
  • DIN EN 10250-4 - Open die steel forgings for general engineering purposes - Part 4: Stainless steels
  • DIN EN 10263-5 - Steel rod, bars and steel wire for cold heading and cold extrusion - Part 5: Technical delivery conditions for stainless steels
  • DIN EN 10272 - Stainless steel bars for pressure purposes
  • DIN EN 10297-2 (2005) - Seamless circular steel tubes for mechanical and general engineering purposes - Technical delivery conditions - Part 2: Stainless steel
  • DIN EN 10088-1 - Stainless steels - Part 1: List of stainless steels
  • DIN EN 10088-2 - Stainless steels - Part 2: Technical delivery conditions for sheet/plate and strip of corrosion resisting steels for general purposes

Steel FE-PM1901 (X12CrNi13) - 600 MPa <= Rm <= 800 MPa - Bars - De <= 70 mm

Chemical composition(wt.%) of 1.4006 grade: to DIN 1654-5 (1989)

Elements Min.(≥) Max.(≤) Similar Remarks
C 0.08 0.15
Si - 1.00
Mn - 1.50
P - 0.040
S 0.15 0.35
Cr 12.0 13.0
Ni - 0.60

1.4006 - Detail

Steel FE-PM1901 (X12CrNi13) - 600 MPa <= Rm <= 800 MPa - Bars - De <= 70 mm 
Stainless steels - Technical delivery conditions for drawn wire 
Stainless steels - Part 1: List of stainless steels 
Ferritic stainless steel

Mechanical properties of grade 1.4006 DIN 1654-5 (1989)

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
192 (≥) 395 (≥) 14 21 44 Solution and Aging, Annealing, Ausaging, Q+T,etc 331

Physical properties of grade 1.4006 DIN 1654-5 (1989)

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
595 (≥) 391 (≥) 41 11 41 Solution and Aging, Annealing, Ausaging, Q+T,etc 132
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
567 536 734

Equivalent Products

We can customize the production of 1.4006 grade, contact us for the best solution.