Seamless circular steel tubes for mechanical and general engineering purposes - Technical delivery conditions - Part 2: Stainless steel
Elements | Min.(≥) | Max.(≤) | Similar | Remarks |
---|---|---|---|---|
C | - | 0.02 | ||
Si | - | 0.70 | ||
Mn | - | 1.00 | ||
P | - | 0.03 | ||
S | - | 0.01 | ||
Cr | 19.50 | 20.50 | ||
Ni | 17.50 | 18.50 | ||
Mo | 6.00 | 7.00 | ||
N | 0.18 | 0.25 | ||
Cu | 0.50 | 1.00 |
Seamless circular steel tubes for mechanical and general engineering purposes - Technical delivery conditions - Part 2: Stainless steel
Proof strength Rp0.2 (MPa) |
Tensile strength Rm (MPa) |
Impact energy KV (J) |
Elongation at fracture A (%) |
Reduction in cross section on fracture Z (%) |
As-Heat-Treated Condition | Brinell hardness (HBW) |
---|---|---|---|---|---|---|
962 (≥) | 522 (≥) | 34 | 24 | 41 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 131 |
Property | Density kg/dm3 |
Temperature T °C/F |
Specific heat J / kgK |
Thermal conductivity W/mK |
Electric resistance µΩ·cm |
Modulus of elasticity kN/mm2 |
Expansion rate |
---|---|---|---|---|---|---|---|
282 (≥) | 526 (≥) | 14 | 34 | 11 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 423 | |
Temp. °C/°F |
Creep strain limit (10000h) (Rp1,0) N/mm2 |
Creep rupture strength (10000h) (Rp1,0) N/mm2 |
|||||
729 | 814 | 664 |
We can customize the production of 1.4547 grade, contact us for the best solution.
–sales@specificsteel.com