X1CrNiMoCuN20-18-7 Stainless Steels to ISO 15510 (2010)

X1CrNiMoCuN20-18-7 - Specification & Application

  • ISO 15510 (2010) - Stainless steels -- Chemical composition
  • ISO 16143-2 (2004) - Stainless steels for general purposes -- Part 2: Semi-finished products, bars, rods and sections
  • ISO 16143-3 (2005) - Stainless steels for general purposes -- Part 3: Wire
  • ISO 9328-7 (2011) - Steel flat products for pressure purposes - Technical delivery conditions - Part 7: Stainless steels
  • ISO/TS 15510 (2003) - Stainless steels - Chemical composition

Stainless steels - Chemical composition

Chemical composition(wt.%) of X1CrNiMoCuN20-18-7 grade: to ISO 15510 (2010)

Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.02
Si - 0.70
Mn - 1.00
P - 0.035
S - 0.015
Cr 19.50 20.50
Ni 17.50 18.50
Mo 6.00 7.00
N 0.18 0.25
Cu 0.50 1.00

X1CrNiMoCuN20-18-7 - Detail

Stainless steels - Chemical composition

Mechanical properties of grade X1CrNiMoCuN20-18-7 ISO 15510 (2010)

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
963 (≥) 411 (≥) 41 32 41 Solution and Aging, Annealing, Ausaging, Q+T,etc 124

Physical properties of grade X1CrNiMoCuN20-18-7 ISO 15510 (2010)

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
383 (≥) 465 (≥) 12 33 23 Solution and Aging, Annealing, Ausaging, Q+T,etc 311
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
965 257 926

Equivalent Products

We can customize the production of X1CrNiMoCuN20-18-7 grade, contact us for the best solution.