9Mn2V Special Alloy

Chemical composition%of the ladle analysis of grade9Mn2V

C(%)Si(%)Mn(%)P(%)S(%)Cr(%)Ni(%)V(%)Cu(%)
0.85~0.95≤0.401.70~2.00≤0.030≤0.030≤0.25≤0.200.10~0.25≤0.30
  • » Alloy steel the performance characteristic and the USES(4)
  • » Alloy steel the performance characteristic and the USES(3)
  • » Alloy steel the performance characteristic and the USES(2)
  • » Alloy steel the performance characteristic and the USES(1)
  • Mechanical properties of grade9Mn2V

    Proof strength
    Rp0.2(MPa)
    Tensile strength
    Rm(MPa)
    Impact energy
    KV(J)
    Elongation at fracture
    A(%)
    Reduction in cross section on fracture
    Z(%)
    As-Heat-Treated Condition Brinell hardness(HBW)
    884(≥) 645(≥) 12 33 42 Solution and Aging,Annealing,Ausaging,Q+T,etc 231

    Physical properties of grade 9Mn2V

    Property Density
    kg/dm3
    Temperature T
    °C/F
    Specific heat
    J/kgK
    Thermal conductivity
    W/mK
    Electric resistance
    µΩ·cm
    Modulus of elasticity
    kN/mm2
    Expansion rate
    367(≥) 762(≥) 43 21 44 Solution and Aging,Annealing,Ausaging,Q+T,etc 324
    Temp.
    °C/°F
    Creep strain limit
    (10000h)
    (Rp1,0)N/mm2
    Creep rupture strength
    (10000h)
    (Rp1,0)N/mm2
    694 543 413

    9Mn2V Range of products

    Product type Products Dimension Processes Deliver Status
    Plates/Sheets Plates/Sheets 0.08-200mm(T)*W*L Forging,hot rolling and cold rolling Annealed,Solution and Aging,Q+T,ACID-WASHED,Shot Blasting
    Steel Bar Round Bar,Flat Bar,Square Bar Φ8-1200mm*L Forging,hot rolling and cold rolling,Cast Black,Rough Turning,Shot Blasting,
    Coil/Strip Steel Coil/Steel Strip 0.03-16.0x1200mm Cold-Rolled&Hot-Rolled Annealed,Solution and Aging,Q+T,ACID-WASHED,Shot Blasting
    Pipes/Tubes Seamless Pipes/Tubes,Welded Pipes/Tubes OD:6-219mm x WT:0.5-20.0mm Hot extrusion,Cold Drawn,Welded Annealed,Solution and Aging,Q+T,ACID-WASHED

    9Mn2V Steel Stock

    Steel grade Dimension Shape Unit Quantity Delivery state Query
    SkD-11 Round Bar Stock Φ30-Φ350 Round Bar Kgs 3102 Hot-Rolled+Annealed+black Enquiry
    17-4PH Coil Stock 0.08*200mm Coil or Strip Kgs 1623 Cold-Rolled+Annealed Enquiry
    D2 Round bar Φ25-Φ380mm Round Bar Kgs 45325 Hot-Rolled+Annealed+black Enquiry
    Cr8 flat bar 12*355*L Flat or Square bar Kgs 3965 Forged+Annealed+black Enquiry
    17-4PH Round Bar Φ5-300mm*L Round Bar Kgs 46958 Hot-Rolled+Annealed+black Enquiry
    17-4PH plate 8-45*1200*3000mm Plate or Sheet Tons 4.9 Hot-Rolled+Annealed+black Enquiry
    Cr12MoV 12-160(T)*310-610(W)*L Plate or Sheet Tons 12.38 Hot-Rolled+Annealed+black Enquiry
    1.2601 12-160(T)*310-610(W)*L Plate or Sheet Tons 11.22 Hot-Rolled+Annealed+black Enquiry
    IncoloyA-286 / GH 2132 Stock Φ8-65mm*L Round Bar Kgs 489 Hot-Rolled+Annealed+black Enquiry
    Incoloy800 round bar Φ115*1400 Round Bar Kgs 169 Hot-Rolled+Annealed+black Enquiry
    17-7PH / 631 Coil & Strip, Sheet Stock 0.3-3.0*10-180mm Coil or Strip Kgs 1236.22 Cold-Rolled+Annealed Enquiry
    X22CrMoV12-1 / 1.4923 Φ17mm Round Bar Kgs 300 Hot-Rolled+Annealed+black Enquiry
    1.2083 Forged Plate T:105-185mm*W:510*L Plate or Sheet Tons 26 Forged+QT Enquiry
    X22CrMoV12-1 / 1.4923 Φ30mm Round Bar Kgs 300 Hot-Rolled+Annealed+black Enquiry
    1.4882 strip/sheet/plate stock 3.5x200x1000-2000mm Coil or Strip Kgs 200 Cold-Rolled+Annealed Enquiry
    A387 F5 & Grade 5 sheet Coil strip 0.5mmx200mmxC Coil or Strip Tons 3 Cold-Rolled+Annealed Enquiry
    A387 F5 & Grade 5 Hot Coil stock Select Tons 3 Hot-Rolled+Annealed+black Enquiry
    T45Cr5Si3 Round Bar Dia.40mm Round Bar Kgs 500 Hot-Rolled+Annealed+black Enquiry
    UNS K30960(VIM+ESR) Bright Round Bar Dia.22mm Round Bar Kgs 50 Hot-Rolled+Annealed+black Enquiry
    SA-437 Grade B4B/SUS 616 /422 Forged Bar Dia.160xL Round Bar Kgs 2120 Forged+QT Enquiry