A 240 S30403 Stainless Steels to A 240/A 240M (2012)

A 240 S30403 - Specification & Application

  • A 240/A 240M (2012) - Chromium and Chromium-Nickel Stainless Steel Plate, Sheet, and Strip for Pressure Vessels and for General Applications

Chromium and Chromium-Nickel Stainless Steel Plate, Sheet, and Strip for Pressure Vessels and for General Applications

Chemical composition(wt.%) of A 240 S30403 grade: to A 240/A 240M (2012)

Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.03
Si - 1.00
Mn - 2.00
P - 0.045
S - 0.03
Cr 18.0 20.0
Ni 8.00 12.0

A 240 S30403 - Detail

A 240/A 240M (2012) Chromium and Chromium-Nickel Stainless Steel Plate, Sheet, and Strip for Pressure Vessels and for General Applications  
Austenitic (Chromium-Nickel) (Chromium-Manganese-Nickel)

Mechanical properties of grade A 240 S30403 A 240/A 240M (2012)

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
726 (≥) 859 (≥) 31 41 14 Solution and Aging, Annealing, Ausaging, Q+T,etc 323

Physical properties of grade A 240 S30403 A 240/A 240M (2012)

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
428 (≥) 525 (≥) 44 42 31 Solution and Aging, Annealing, Ausaging, Q+T,etc 112
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
589 884 931