A 646 Grade HP 9-4-30 Stainless Steels to A 646/A 646M (2011)

A 646 Grade HP 9-4-30 - Specification & Application

  • A 646/A 646M (2011) - Premium Quality Alloy Steel Blooms and Billets for Aircraft and Aerospace Forgings

Premium Quality Alloy Steel Blooms and Billets for Aircraft and Aerospace Forgings

Chemical composition(wt.%) of A 646 Grade HP 9-4-30 grade: to A 646/A 646M (2011)

Elements Min.(≥) Max.(≤) Similar Remarks
C 0.29 0.34
Si - 0.10
Mn 0.10 0.35
Ni 7.00 8.00
Cr 0.90 1.10
Al - -
Cu - -
Ti - -
Fe - -
Mo 0.90 1.10
Co 4.25 4.75
V 0.06 0.12
P - 0.01
S - 0.01

A 646 Grade HP 9-4-30 - Detail

Premium Quality Alloy Steel Blooms and Billets for Aircraft and Aerospace Forgings

Mechanical properties of grade A 646 Grade HP 9-4-30 A 646/A 646M (2011)

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
384 (≥) 687 (≥) 13 32 42 Solution and Aging, Annealing, Ausaging, Q+T,etc 324

Physical properties of grade A 646 Grade HP 9-4-30 A 646/A 646M (2011)

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
815 (≥) 938 (≥) 31 42 32 Solution and Aging, Annealing, Ausaging, Q+T,etc 212
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
893 817 831

Equivalent Products