HEV2 Stainless Steels

HEV2 - Specification & Application

Steel for exhaust valves

Chemical composition(wt.%) of HEV2 grade:

Elements Min.(≥) Max.(≤) Similar Remarks
C 0.04 -
Si 0.08 -
Mn 2.25 -
P - -
S - -
Cr 16.0 -
Ni - remaining

HEV2 - Detail

Steel for exhaust valves

Mechanical properties of grade HEV2

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
963 (≥) 593 (≥) 44 14 21 Solution and Aging, Annealing, Ausaging, Q+T,etc 231

Physical properties of grade HEV2

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
867 (≥) 385 (≥) 41 21 14 Solution and Aging, Annealing, Ausaging, Q+T,etc 231
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
918 924 513

Equivalent Products

We can customize the production of HEV2 grade, contact us for the best solution.