Steel Sheet, Strip, and Plate 0,48Cr - 8,0Ni - 4,0Co - 4,48Mo - 0,09V - (0,24 - 0,30C) Consumable Electrode Melted, Annealed
Elements | Min.(≥) | Max.(≤) | Similar | Remarks |
---|---|---|---|---|
C | 0.24 | 0.30 | ||
Si | - | 0.10 | ||
Mn | 0.10 | 0.35 | ||
Ni | 7.00 | 9.00 | ||
Cr | 0.35 | 0.60 | ||
Al | - | - | ||
Cu | - | - | ||
Ti | - | - | ||
Fe | - | - | ||
Mo | 0.35 | 0.60 | ||
Co | 3.50 | 4.50 | ||
V | 0.06 | 0.12 | ||
P | - | 0.01 | ||
S | - | 0.01 |
Steel Sheet, Strip, and Plate 0,48Cr - 8,0Ni - 4,0Co - 4,48Mo - 0,09V - (0,24 - 0,30C) Consumable Electrode Melted, Annealed
Proof strength Rp0.2 (MPa) |
Tensile strength Rm (MPa) |
Impact energy KV (J) |
Elongation at fracture A (%) |
Reduction in cross section on fracture Z (%) |
As-Heat-Treated Condition | Brinell hardness (HBW) |
---|---|---|---|---|---|---|
113 (≥) | 928 (≥) | 13 | 32 | 31 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 323 |
Property | Density kg/dm3 |
Temperature T °C/F |
Specific heat J / kgK |
Thermal conductivity W/mK |
Electric resistance µΩ·cm |
Modulus of elasticity kN/mm2 |
Expansion rate |
---|---|---|---|---|---|---|---|
561 (≥) | 857 (≥) | 33 | 24 | 13 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 131 | |
Temp. °C/°F |
Creep strain limit (10000h) (Rp1,0) N/mm2 |
Creep rupture strength (10000h) (Rp1,0) N/mm2 |
|||||
463 | 271 | 267 |
We can customize the production of HP 9-4-25 grade, contact us for the best solution.