HP 9-4-30 Stainless Steels to SAE AMS 6524E (1991)

HP 9-4-30 - Specification & Application

  • SAE AMS 6524E (1991) - Steel, Sheet, Strip, and Plate 1.0Cr - 7.5Ni - 4.5Co - 1.0Mo - 0.09V (0.29 - 0.34C) Consumable Electrode Vacuum Melted, Annealed

Steel, Sheet, Strip, and Plate 1.0Cr - 7.5Ni - 4.5Co - 1.0Mo - 0.09V (0.29 - 0.34C) Consumable Electrode Vacuum Melted, Annealed

Chemical composition(wt.%) of HP 9-4-30 grade: to SAE AMS 6524E (1991)

Elements Min.(≥) Max.(≤) Similar Remarks
C 0.29 0.34
Si - 0.10
Mn 0.10 0.35
Ni 7.00 8.00
Cr 0.90 1.10
Al - -
Cu - -
Ti - -
Fe - -
Mo 0.90 1.10
Co 4.25 4.75
V 0.06 0.12
P - 0.01
S - 0.01

HP 9-4-30 - Detail

Steel, Sheet, Strip, and Plate 1.0Cr - 7.5Ni - 4.5Co - 1.0Mo - 0.09V (0.29 - 0.34C) Consumable Electrode Vacuum Melted, Annealed

Mechanical properties of grade HP 9-4-30 SAE AMS 6524E (1991)

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
782 (≥) 251 (≥) 41 21 24 Solution and Aging, Annealing, Ausaging, Q+T,etc 144

Physical properties of grade HP 9-4-30 SAE AMS 6524E (1991)

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
992 (≥) 961 (≥) 42 44 32 Solution and Aging, Annealing, Ausaging, Q+T,etc 443
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
126 762 583

Equivalent Products

We can customize the production of HP 9-4-30 grade, contact us for the best solution.
sales@specificsteel.com