1.4418 Stainless Steels to SA/EN 10028-7

1.4418 - Specification & Application

  • SA/EN 10028-7 - Specification for flat products made of steels for pressure purposes - Part 7: Stainless steels

Specification for flat products made of steels for pressure purposes - Part 7: Stainless steels

Chemical composition(wt.%) of 1.4418 grade: to SA/EN 10028-7

Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.20
Si - 0.50
Mn - 1.00
P - -
S - -
Ni - -
Cr - 12.50
Al - -
Cu - -
Ti - -
Fe - remaining
N - -
Mo - -
W - 3.00

1.4418 - Detail

Specification for flat products made of steels for pressure purposes - Part 7: Stainless steels

Mechanical properties of grade 1.4418 SA/EN 10028-7

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
651 (≥) 653 (≥) 32 24 41 Solution and Aging, Annealing, Ausaging, Q+T,etc 213

Physical properties of grade 1.4418 SA/EN 10028-7

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
775 (≥) 336 (≥) 23 24 34 Solution and Aging, Annealing, Ausaging, Q+T,etc 322
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
232 128 266

Equivalent Products

We can customize the production of 1.4418 grade, contact us for the best solution.
sales@specificsteel.com