420S29 Special Alloy

Chemical composition%of the ladle analysis of grade420S29

C(%)Si(%)Mn(%)P(%)S(%)Cr(%)Ni(%)
0.14-0.20 Max 1.00Max 1.00Max 0.04Max 0.0311.5-13.5Max 1.00
420S29

Mechanical properties of grade420S29

Proof strength
Rp0.2(MPa)
Tensile strength
Rm(MPa)
Impact energy
KV(J)
Elongation at fracture
A(%)
Reduction in cross section on fracture
Z(%)
As-Heat-Treated Condition Brinell hardness(HBW)
964(≥) 255(≥) 14 33 21 Solution and Aging,Annealing,Ausaging,Q+T,etc 223

Physical properties of grade 420S29

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J/kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
383(≥) 971(≥) 13 41 33 Solution and Aging,Annealing,Ausaging,Q+T,etc 242
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0)N/mm2
Creep rupture strength
(10000h)
(Rp1,0)N/mm2
753 737 446

420S29 Range of products

Product type Products Dimension Processes Deliver Status
Plates/Sheets Plates/Sheets 0.08-200mm(T)*W*L Forging,hot rolling and cold rolling Annealed,Solution and Aging,Q+T,ACID-WASHED,Shot Blasting
Steel Bar Round Bar,Flat Bar,Square Bar Φ8-1200mm*L Forging,hot rolling and cold rolling,Cast Black,Rough Turning,Shot Blasting,
Coil/Strip Steel Coil/Steel Strip 0.03-16.0x1200mm Cold-Rolled&Hot-Rolled Annealed,Solution and Aging,Q+T,ACID-WASHED,Shot Blasting
Pipes/Tubes Seamless Pipes/Tubes,Welded Pipes/Tubes OD:6-219mm x WT:0.5-20.0mm Hot extrusion,Cold Drawn,Welded Annealed,Solution and Aging,Q+T,ACID-WASHED

420S29 Steel Stock

Steel grade Dimension Shape Unit Quantity Delivery state Query
Cr12MoV 12-160(T)*310-610(W)*L Plate or Sheet Tons 12.38 Hot-Rolled+Annealed+black Enquiry
1.2601 12-160(T)*310-610(W)*L Plate or Sheet Tons 11.22 Hot-Rolled+Annealed+black Enquiry
X22CrMoV12-1 / 1.4923 Φ17mm Round Bar Kgs 300 Hot-Rolled+Annealed+black Enquiry
X22CrMoV12-1 / 1.4923 Φ30mm Round Bar Kgs 300 Hot-Rolled+Annealed+black Enquiry
1.2344(H13/X40CrMoV5-1/Z40CDV5) Stock List Dia.182mm - Dia.510mm Round Bar Tons 120 Forged+Annealed+black Enquiry
1.2714 Hot-Work Mould Steel Flat Bar Stock(2019-09-03) Select 0 Select Enquiry
1.2714 Stock list 2020-06-15 Select 0 Select Enquiry
1.2714 QT Bar Stock List 2020-06-15 Select 0 Select Enquiry
1Cr11Ni2W2MoV,961,13Cr11Ni2W2MoV Sheet Select 0 Select Enquiry