Chemical composition(wt.%) of A 176 S42200 grade: to A 176 (2009)

Elements Min.(≥) Max.(≤) Similar Remarks
C 0.20 0.25
Mn - 1.00
Si - 0.75
P - 0.04
S - 0.03
Cr 11.50 13.50
Ni 0.50 1.00
Mo 0.75 1.25
V 0.15 0.30
W 0.75 1.25

A 176 S42200 - Detail

Stainless and Heat-Resisting Chromium Steel Plate, Sheet, and Strip

Mechanical properties of grade A 176 S42200 A 176 (2009)

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
383 (≥) 962 (≥) 42 32 21 Solution and Aging, Annealing, Ausaging, Q+T,etc 241

Physical properties of grade A 176 S42200 A 176 (2009)

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
429 (≥) 734 (≥) 33 23 13 Solution and Aging, Annealing, Ausaging, Q+T,etc 443
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
987 197 274
We can customize the production of A 176 S42200 grade, contact us for the best solution.