A 314 S50100 Stainless Steels to A 314 (2013)

A 314 S50100 - Specification & Application

  • A 314 (2013) - Stainless Steel Billets and Bars for Forging

Stainless Steel Billets and Bars for Forging

Chemical composition(wt.%) of A 314 S50100 grade: to A 314 (2013)

Elements Min.(≥) Max.(≤) Similar Remarks
C 0.10 -
Mn - 1.00
Si - 1.00
P - 0.04
S - 0.03
Cr 4.00 6.00
Ni - -
Mo 0.40 0.65

A 314 S50100 - Detail

Stainless Steel Billets and Bars for Forging

Mechanical properties of grade A 314 S50100 A 314 (2013)

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
696 (≥) 625 (≥) 12 32 44 Solution and Aging, Annealing, Ausaging, Q+T,etc 322

Physical properties of grade A 314 S50100 A 314 (2013)

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
581 (≥) 432 (≥) 11 24 14 Solution and Aging, Annealing, Ausaging, Q+T,etc 244
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
662 558 166

Equivalent Products

We can customize the production of A 314 S50100 grade, contact us for the best solution.