A 358 S32100 Stainless Steels to A 358/A 358M (2008)

A 358 S32100 - Specification & Application

  • A 358/A 358M (2008) - Electric-Fusion-Welded Austenitic Chromium-Nickel Stainless Steel Pipe for High-Temperature Service and General Applications

Electric-Fusion-Welded Austenitic Chromium-Nickel Stainless Steel Pipe for High-Temperature Service and General Applications

Chemical composition(wt.%) of A 358 S32100 grade: to A 358/A 358M (2008)

Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.08
Mn - 2.00
Si - 1.00
P - 0.045
S - 0.03
Cr 17.00 19.00
Ni 9.00 12.00
N - 0.10

A 358 S32100 - Detail

Electric-Fusion-Welded Austenitic Chromium-Nickel Stainless Steel Pipe for High-Temperature Service and General Applications

Mechanical properties of grade A 358 S32100 A 358/A 358M (2008)

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
521 (≥) 673 (≥) 44 31 41 Solution and Aging, Annealing, Ausaging, Q+T,etc 241

Physical properties of grade A 358 S32100 A 358/A 358M (2008)

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
738 (≥) 844 (≥) 43 12 23 Solution and Aging, Annealing, Ausaging, Q+T,etc 423
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
119 151 693
We can customize the production of A 358 S32100 grade, contact us for the best solution.