A 479 S20161 Stainless Steels to A 479/A 479M (2013)

A 479 S20161 - Specification & Application

  • A 479/A 479M (2013) - Stainless Steel Bars and Shapes for Use in Boilers and Other Pressure Vessels

Stainless Steel Bars and Shapes for Use in Boilers and Other Pressure Vessels

Chemical composition(wt.%) of A 479 S20161 grade: to A 479/A 479M (2013)

Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.15
Mn 4.00 6.00
Si 3.00 4.00
P - 0.04
S - 0.04
Cr 15.00 18.00
Ni 4.00 6.00
Mo - 0.50
N 0.08 0.20

A 479 S20161 - Detail

Stainless Steel Bars and Shapes for Use in Boilers and Other Pressure Vessels

Mechanical properties of grade A 479 S20161 A 479/A 479M (2013)

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
432 (≥) 449 (≥) 24 43 14 Solution and Aging, Annealing, Ausaging, Q+T,etc 122

Physical properties of grade A 479 S20161 A 479/A 479M (2013)

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
475 (≥) 441 (≥) 34 12 13 Solution and Aging, Annealing, Ausaging, Q+T,etc 233
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
898 696 935

Equivalent Products

We can customize the production of A 479 S20161 grade, contact us for the best solution.