F 899 S20161 Stainless Steels to F 899 (2012)

F 899 S20161 - Specification & Application

  • F 899 (2012) - Standard Specification for Wrought Stainless Steels for Surgical Instruments

Standard Specification for Wrought Stainless Steels for Surgical Instruments

Chemical composition(wt.%) of F 899 S20161 grade: to F 899 (2012)

Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.15
Mn 4.00 6.00
Si 3.00 4.00
P - 0.04
S - 0.04
Cr 15.00 18.00
Ni 4.00 6.00
Mo - 0.50
N 0.08 0.20

F 899 S20161 - Detail

Standard Specification for Wrought Stainless Steels for Surgical Instruments

Mechanical properties of grade F 899 S20161 F 899 (2012)

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
747 (≥) 574 (≥) 14 24 13 Solution and Aging, Annealing, Ausaging, Q+T,etc 233

Physical properties of grade F 899 S20161 F 899 (2012)

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
534 (≥) 196 (≥) 32 11 34 Solution and Aging, Annealing, Ausaging, Q+T,etc 412
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
167 171 765

Equivalent Products

We can customize the production of F 899 S20161 grade, contact us for the best solution.
sales@specificsteel.com