Martensitic Stainless Steel Bars for High-Temperature Service
Elements | Min.(≥) | Max.(≤) | Similar | Remarks |
---|---|---|---|---|
C | 0.27 | 0.32 | ||
Si | - | 0.50 | ||
Mn | 0.95 | 1.35 | ||
P | - | 0.025 | ||
S | - | 0.025 | ||
Cr | 11.0 | 12.0 | ||
Ni | - | 0.50 | ||
Mo | 2.50 | 3.00 | ||
V | 0.20 | 0.30 |
Martensitic Stainless Steel Bars for High-Temperature Service
Proof strength Rp0.2 (MPa) |
Tensile strength Rm (MPa) |
Impact energy KV (J) |
Elongation at fracture A (%) |
Reduction in cross section on fracture Z (%) |
As-Heat-Treated Condition | Brinell hardness (HBW) |
---|---|---|---|---|---|---|
659 (≥) | 894 (≥) | 41 | 33 | 31 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 322 |
Property | Density kg/dm3 |
Temperature T °C/F |
Specific heat J / kgK |
Thermal conductivity W/mK |
Electric resistance µΩ·cm |
Modulus of elasticity kN/mm2 |
Expansion rate |
---|---|---|---|---|---|---|---|
738 (≥) | 629 (≥) | 33 | 34 | 11 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 411 | |
Temp. °C/°F |
Creep strain limit (10000h) (Rp1,0) N/mm2 |
Creep rupture strength (10000h) (Rp1,0) N/mm2 |
|||||
896 | 939 | 829 |
We can customize the production of A 565 619 grade, contact us for the best solution.