  • A 565/A 565M (2010) - Martensitic Stainless Steel Bars for High-Temperature Service

Martensitic Stainless Steel Bars for High-Temperature Service

Chemical composition(wt.%) of A 565 619 grade: to A 565/A 565M (2010)

Elements Min.(≥) Max.(≤) Similar Remarks
C 0.27 0.32
Si - 0.50
Mn 0.95 1.35
P - 0.025
S - 0.025
Cr 11.0 12.0
Ni - 0.50
Mo 2.50 3.00
V 0.20 0.30

A 565 619 - Detail

Martensitic Stainless Steel Bars for High-Temperature Service

Mechanical properties of grade A 565 619 A 565/A 565M (2010)

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
984 (≥) 196 (≥) 22 32 21 Solution and Aging, Annealing, Ausaging, Q+T,etc 442

Physical properties of grade A 565 619 A 565/A 565M (2010)

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
443 (≥) 673 (≥) 31 12 24 Solution and Aging, Annealing, Ausaging, Q+T,etc 333
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
477 674 161

Equivalent Products

We can customize the production of A 565 619 grade, contact us for the best solution.