A 988 S41026 Stainless Steels to A 988/A 988M (2011)

A 988 S41026 - Specification & Application

  • A 988/A 988M (2011) - Hot Isostatically-Pressed Stainless Steel Flanges, Fittings, Valves, and Parts for High Temperature Service

Hot Isostatically-Pressed Stainless Steel Flanges, Fittings, Valves, and Parts for High Temperature Service

Chemical composition(wt.%) of A 988 S41026 grade: to A 988/A 988M (2011)

Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.15
Mn - 1.00
Si - 1.00
P - 0.02
S - 0.02
Cr 11.50 13.50
Ni 1.00 2.00
Mo 0.40 0.60
Cu - 0.50

A 988 S41026 - Detail

Hot Isostatically-Pressed Stainless Steel Flanges, Fittings, Valves, and Parts for High Temperature Service

Mechanical properties of grade A 988 S41026 A 988/A 988M (2011)

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
789 (≥) 261 (≥) 22 14 22 Solution and Aging, Annealing, Ausaging, Q+T,etc 423

Physical properties of grade A 988 S41026 A 988/A 988M (2011)

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
529 (≥) 253 (≥) 42 24 21 Solution and Aging, Annealing, Ausaging, Q+T,etc 232
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
965 447 669

Equivalent Products

We can customize the production of A 988 S41026 grade, contact us for the best solution.
sales@specificsteel.com