ASTMXM-13 Stainless Steels

ASTMXM-13 - Specification & Application

ASTMXM-13

Chemical composition(wt.%) of ASTMXM-13 grade:

Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.05
Si - 0.01
Mn - 0.02
P - 0.01
S - 0.008
Cr 12.25 13.0
Ni 7.50 8.50
Mo 2.00 2.50
Al 0.90 1.35
N - 0.01

ASTMXM-13 - Detail

ASTMXM-13

Mechanical properties of grade ASTMXM-13

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
459 (≥) 487 (≥) 13 44 43 Solution and Aging, Annealing, Ausaging, Q+T,etc 343

Physical properties of grade ASTMXM-13

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
497 (≥) 429 (≥) 22 41 22 Solution and Aging, Annealing, Ausaging, Q+T,etc 122
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
972 627 174
We can customize the production of ASTMXM-13 grade, contact us for the best solution.
sales@specificsteel.com