S42200 Special Alloy

Chemical composition%of the ladle analysis of gradeS42200

C(%)Si(%)Mn(%)P(%)S(%)Cr(%)Ni(%)Mo(%)V(%)W(%)Cu(%)Other(%)
0.20-0.250.20-0.601.00.040 0.03011.0-13.50.50-1.00.75-1.250.17-0.300.75-1.250.50Fe:Balance;
UNS S42200 is a hardenable stainless steel designed for use at temperatures of up to 1200ºF (649ºC). UNS S42200 has good resistance to scaling and oxidation. Through heat treatment, high mechanical properties can be developed. UNS S42200 is used in applications such as compressors or steam turbines and also in aircraft parts, valves, high temperature bolting etc. 

Mechanical properties of gradeS42200

Proof strength
Rp0.2(MPa)
Tensile strength
Rm(MPa)
Impact energy
KV(J)
Elongation at fracture
A(%)
Reduction in cross section on fracture
Z(%)
As-Heat-Treated Condition Brinell hardness(HBW)
662(≥) 269(≥) 42 12 11 Solution and Aging,Annealing,Ausaging,Q+T,etc 122

Physical properties of grade S42200

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J/kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
787(≥) 668(≥) 42 24 14 Solution and Aging,Annealing,Ausaging,Q+T,etc 221
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0)N/mm2
Creep rupture strength
(10000h)
(Rp1,0)N/mm2
149 343 566

S42200 Range of products

Product type Products Dimension Processes Deliver Status
Plates/Sheets Plates/Sheets 0.08-200mm(T)*W*L Forging,hot rolling and cold rolling Annealed,Solution and Aging,Q+T,ACID-WASHED,Shot Blasting
Steel Bar Round Bar,Flat Bar,Square Bar Φ8-1200mm*L Forging,hot rolling and cold rolling,Cast Black,Rough Turning,Shot Blasting,
Coil/Strip Steel Coil/Steel Strip 0.03-16.0x1200mm Cold-Rolled&Hot-Rolled Annealed,Solution and Aging,Q+T,ACID-WASHED,Shot Blasting
Pipes/Tubes Seamless Pipes/Tubes,Welded Pipes/Tubes OD:6-219mm x WT:0.5-20.0mm Hot extrusion,Cold Drawn,Welded Annealed,Solution and Aging,Q+T,ACID-WASHED

S42200 Steel Stock

Steel grade Dimension Shape Unit Quantity Delivery state Query
Stainless Steel 422 / Alloy 422 AMS 5655 UNS S42200/616/B4B Round Bar Stock Select 0 Select Enquiry