NV8 Stainless Steels

NV8 - Specification & Application

Steel for intake valves

Chemical composition(wt.%) of NV8 grade:

Elements Min.(≥) Max.(≤) Similar Remarks
C 0.35 0.45
Si 3.60 4.20
Mn 0.20 0.40
P - 0.030
S - 0.04
Cr 1.85 2.50
Ni - 0.10
Mo - O.25
Cu - 0.25

NV8 - Detail

Steel for intake valves

Mechanical properties of grade NV8

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
914 (≥) 951 (≥) 23 31 12 Solution and Aging, Annealing, Ausaging, Q+T,etc 314

Physical properties of grade NV8

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
625 (≥) 613 (≥) 21 22 13 Solution and Aging, Annealing, Ausaging, Q+T,etc 223
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
517 578 169

Equivalent Grade

Equivalent Products

We can customize the production of NV8 grade, contact us for the best solution.