Sheet and Strip 15Cr - 8,4Ni - 2,2Mo - 1,1Al, vac. Induct. Melted, Solution Heat Treated
Elements | Min.(≥) | Max.(≤) | Similar | Remarks |
---|---|---|---|---|
C | - | 0.05 | ||
Si | - | - | ||
Mn | - | - | ||
Cr | 13.50 | 15.50 | ||
Ni | 7.50 | 9.50 | ||
Mo | 2.00 | 3.00 | ||
Co | - | - | ||
W | - | - | ||
Al | 0.75 | 1.50 | ||
Cu | - | - | ||
Ti | - | - | ||
Fe | - | - |
Sheet and Strip 15Cr - 8,4Ni - 2,2Mo - 1,1Al, vac. Induct. Melted, Solution Heat Treated
Proof strength Rp0.2 (MPa) |
Tensile strength Rm (MPa) |
Impact energy KV (J) |
Elongation at fracture A (%) |
Reduction in cross section on fracture Z (%) |
As-Heat-Treated Condition | Brinell hardness (HBW) |
---|---|---|---|---|---|---|
212 (≥) | 733 (≥) | 42 | 42 | 34 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 343 |
Property | Density kg/dm3 |
Temperature T °C/F |
Specific heat J / kgK |
Thermal conductivity W/mK |
Electric resistance µΩ·cm |
Modulus of elasticity kN/mm2 |
Expansion rate |
---|---|---|---|---|---|---|---|
497 (≥) | 633 (≥) | 42 | 44 | 23 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 411 | |
Temp. °C/°F |
Creep strain limit (10000h) (Rp1,0) N/mm2 |
Creep rupture strength (10000h) (Rp1,0) N/mm2 |
|||||
518 | 155 | 462 |
We can customize the production of PH 14-8 Mo grade, contact us for the best solution.
–sales@specificsteel.com