Chemical composition(wt.%) of S45500 grade:

Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.50
Mn - 0.50
Si - 0.50
P - 0.04
S - 0.03
Cr 11.00 12.50
Ni 7.50 9.50
Mo - 0.50

S45500 - Detail

Stainless Steel (Custom 455)

Mechanical properties of grade S45500

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
125 (≥) 857 (≥) 12 24 32 Solution and Aging, Annealing, Ausaging, Q+T,etc 143

Physical properties of grade S45500

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
862 (≥) 714 (≥) 42 14 12 Solution and Aging, Annealing, Ausaging, Q+T,etc 221
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
181 853 556